Slow stress corrosion testing machine
The microcomputer controlled electronic slow strain stress corrosion testing machine is mainly used for detecting and studying the mechanical properti
Product details

1、 Product Introduction

The YLW-10 microcomputer controlled slow tensile stress corrosion testing machine is a product developed by our company. It uses a stepper motor as the power source to drive precision ball screws for loading, and adopts the company's self-developed electronic testing machine closed-loop measurement and control system for fully automatic control of the machine. It has the characteristics of simple structure, low noise, high control accuracy, and simple operation. Mainly used for testing and studying the mechanical properties of metal materials such as static tensile strength, creep, stress corrosion, etc. It can be used in NaOH, NO3, H2S, CL solutions, methanol, etc N2O4、NH3、 The stress corrosion damage characteristics test of metals in humid air and water media environment can dynamically display the load, deformation, velocity, time and test curve in real time during the loading process. After the test is completed, the test results can be automatically saved, queried and printed, and the data during the test process can be exported.

IISlow stress corrosion testing machineProduct Features

1. Equipped with a remote control box, it can achieve fast/slow movement adjustment of the actuator head, with flexible operation and easy switching;

2. Having the function of returning to the initial position after the experiment is completed, intelligent, efficient, and fast;

3. Equipped with limit protection and overload/overcurrent protection for the largest working position, reliable and safe;

4. Build a powerful experimental database, where experimental data can be saved, queried, and accessed at any time;

5. It can achieve various control methods such as constant rate force control, constant rate stress control, constant rate deformation control, constant rate strain control, constant rate displacement control, force holding, deformation holding, displacement holding, and user programmable control;

6. Multiple test curves can be switched and displayed: stress-strain curve, force deformation curve, force displacement curve, force time curve, deformation time curve, displacement time curve, and stress-strain curve. Partial amplification of experimental curves, comparison of multiple curve superposition;

7. Can work continuously without faults for more than one month, and can continue the test on the basis of the original test after power failure recovery.

3、 Main technical parameters and indicators

Serial Number

Inspection items

technical requirement

1

The most powerful experimental force

10KN 20KN 50KN 100KN can be selected

2

Test force resolution

1/200000

3

Relative error of indication value

± 1% within the range of 1% -100%

4

Test force indication repeatability relative error

≤1%

5

Loading speed range

0.001N/s-50N/s

6

Displacement velocity range

10-6Mm/min to 1mm/min

7

The biggest itinerary

50mm

8

loading method

electric

9

Power supply voltage(There must be reliable grounding measures

~220V±10% 50Hz

10

Motor Power

80W

4、 Product features:

1. Automatic tracking measurement: using electronic force measurement and high-precision sensors to ensure measurement accuracy;
2. High resolution measurement: The overall resolution of the experiment is *, and there is no grading;
3. Automatic data processing: After the experiment is completed, the system automatically processes the data according to standard requirements;
4. Software zeroing: Press the zeroing button, and the displayed value will automatically reset to zero;
5. Digital display: Full digital display of test force value, test rate, time, temperature, and test curve;
6. Peak retention: Maintain the peak value after the experiment is completed;
7. Automatic protection: Automatically implement overload, fracture, and displacement protection, and automatically record fracture time;
8. Automatic printing: After the experiment is completed, the test report and test curve can be automatically printed out,
Record and output two sets of test data and curve graphs for stress-strain and self corrosion potential time. And it can record and calculate the fracture life, tensile strength, cross-sectional shrinkage rate, strain, elongation of the specimen, and stress-strain integral (physical meaning is the work done by external forces on the specimen);

5、 Product Configuration Checklist:

1. One microcomputer controlled electronic slow strain stress corrosion testing machine host
2. A set of digital microcomputer controlled slow strain stress corrosion test control system
3. One microcomputer controlled slow strain stress corrosion test control system software (CD)
4. One high-precision force sensor
5. A set of digital displacement sensors
6. Two sets of stress corrosion environment medium pools
7. One set of test fixtures (two types of threaded connections and one set of pin connections)
8. One branded computer
9. One A4 color inkjet printer

Online inquiry
  • Contacts
  • Company
  • Telephone
  • Email
  • WeChat
  • Verification Code
  • Message Content

Successful operation!

Successful operation!

Successful operation!